In the 1950s, the SherrittGordon ammonia pressureleaching process for nickel was introduced. In this process, nickel sulfide flotation concentrates are reacted under pressure with oxygen together with ammonia, which helps to facilitate the dissolution by forming soluble nickelammonia complex ions.